Typical Chemical Analysis of HPDA® Certificate of Quality
| Hydrogen Concentration in Sapphire IR analysis NMR analysis CZ method, from Vernuil crackles, top <0.2ppm CZ method, from Vernuil crackles, center <0.2ppm 2560ppm CZ method, from Vernuil crackles, bottom 0.3ppm 919ppm CZ method, from EMT HPDA® crackles 0.3ppm 243ppm Kyropoulos, Vernuil crackles, top <0.2ppm Kyropoulos, Vernuil crackles, center <0.2ppm 635ppm Kyropoulos, Vernuil crackles, bottom <0.2ppm Kyropoulos, EMT HPDA®, top <0.2ppm Kyropoulos, EMT HPDA®, center <0.2ppm 355ppm Kyropoulos, EMT HPDA®, bottom <0.2ppm HEM method, from EMT HPDA® crackles <0.2ppm 410ppm HEM method, from Vernuil crackles 12ppm 807ppm Vernuil, Spolchene 2.3ppm 1078ppm EMT HPDA® 27ppm Quartz ( certificate ~800 ppm OH) 1300ppm 346ppm Muscovit mineral used as standard for NMR 40000ppm IR transmission is given for samples with the thickness of 10mm |